2. sorting
U1-Chrom
Second-quality item, - the product may have minor cosmetic imperfections such as small scratches, marks, or minor dents.
In some cases, a narrow strip of superficial corrosion may be present on the aluminum back plate at the joint. This is caused by a galvanic reaction that can occur if the packaging has absorbed salt-laden moisture during transport. The corrosion is purely superficial and can be completely removed with approximately two minutes of sanding using 800-grit sandpaper, optionally followed by a few minutes of polishing. (See photos)
With small marks
VZ50, MS50, Florida, Dakota (Not for MS50 Super)
30mm pipe